- The proper moment for casting is clearly recognisable and the excellent melting properties of the alloy ensure reliable filling of the mould.
- The lower mould preheating temperature of only 800 °C (1472 °F) gives a very smooth surface.
- The lower casting temperature of only 1350 °C (2462 °F) reduces the reactionof the alloy with the investment material.
- The oxide of Wiron® light is considerably lighter in colour compared to conventional NiCr alloys and is very easy and fast to remove.
...
|
|
|
|
| Wiron® light |
1 pack = 1000 g |
50270 |
| Wiron® light |
1 pack = 250 g |
50272 |
|
|
|