Wirobond C

Chrome cobalt metal-ceramic alloy - nickel-free, beryllium-free

Chrome cobalt metal-ceramic alloy - nickel-free, beryllium-free

  • Biocompatibility and high corrosion resistance thanks to firmly adhering passive layer
  • Biocompatibility certified
  • Modulus of elasticity double that of precious metals
  • High bonding strength with ceramics
  • High heat resistance
  • Low thermal conductivity
  • Optimised for laser welding
  • Trouble-free processing with BEGO system
  • Constant high level of quality thanks to quality assurance system
  Delivery form REF
Wirobond C 1 pack = 1000 g 50115
Wirobond C 1 pack = 250 g 50116
63,3 - 24,8 - 5,3 - 5,1 - 1,0 - x
BEGO colour code 8
CTE 20-600 °C -
CTE 25-500 °C 14,1 / *14,1
Casting temperature [°C] 1500
Color silver
Density [g/cm³] 8,5
Melting interval [°C] 1360, 1420
Modulus of elasticity [GPa] 225 / *222
Pre-heating temperature [°C] 900-1000
Proof stress [RP 0,2] after casting/firing 415 / *395
Standard ISO 9693 + ISO 22674
Suitability for laser welding ja
Tensile strength [RM] 780
Vickers Hardness [HV10] after casting / firing 315 / *320

*All images are subject to BEGO Bremer Goldschlägerei Wilhelm Herbst GmbH & Co. KG