Wirobond® M+
Milled cobalt-chrome restorations
Chemical composition in % |
---|
Co 63.8 % · Cr 24.8 % · W 5.3 % · Mo 5.1 % · Si 1.0 % |
Alloy characteristics | |
---|---|
Type (according to ISO 22674) | 4 |
Density | 8.6 g/cm³ |
Modulus of elasticity | 235 GPa |
0.2% elongation limit (Rp0.2) | 415 MPa |
Tensile strength (Rm) | 965 MPa |
Hardness (HV 10) | 290 |
Coefficient of thermal expansion (RT – 500°C) | 14.4 10-6 K-1 |
Coefficient of thermal expansion (RT – 600 °C) | 14.6 10-6 K-1 |