Pontonorm

High-gold-content, extra-hard alloy for crowns and bridges, yellow, does not contain palladium, suitable for veneering with low-fusing dental ceramics; biocertificate available.

High-gold-content, extra-hard alloy for crowns and bridges, yellow, does not contain palladium, suitable for veneering with low-fusing dental ceramics; biocertificate available.

  • Extra-hard alloy with a high gold content, compatible with low-fusing porcelains
  Delivery form REF
Pontonorm 61126
73,8 - 9,2 - 9,0 - 4,4 - 2,0 - 1,5 - x
BEGO colour code 4
CTE 20-600 °C 16,8
CTE 25-500 °C 15,8
Casting temperature [°C] 1150
Density [g/cm³] 16,1
Elongation [A5] after casting/firing 5
Elongation [A5] soft -
Elongation [A5] tempered 6
Indications 1, 2, 4, 5, 6
Medium grit size 20
Melting interval [°C] 900 - 980
Modulus of elasticity [GPa] 93
Pre-heating temperature [°C] 700
Proof stress [RP 0,2] after casting/firing 430
Proof stress [RP 0,2] soft -
Proof stress [RP 0,2] tempered 500
Type of alloy extrahart
Vickers Hardness [HV5] after casting / firing 200
Vickers Hardness [HV5] tempered 230
Vickers Hardness[HV5] soft 150