Wirobond® C+

Cobalt-chrome restorations produced with the SLM method

Technical specifications
Chemical composition in %
Co 63.9 % · Cr 24.7 % · W 5.4 % · Mo 5.0 % · Si 1.0 %
Alloy characteristics  
Type (according to ISO 22674) 5
Density 8.6 g/cm³
0.2% elongation limit (Rp0.2) 1,090 MPa
Tensile strength (Rm) 1,315 MPa
Modulus of elasticity 215 GPa
Solidus temperature; liquidus temperature 1,380;1,420°C
Coefficient of thermal expansion (RT – 500°C) 14.3 10-6 K-1
Coefficient of thermal expansion (RT – 600°C) 14.5 10-6 K-1

Images and illustrations are examples; colors, symbols, designs and information on the depicted labels and/or packaging may differ from reality.